Product name |
Plastic hiflow ring |
|||
Material |
PP, PE, PVC, CPVC, PVDF, etc |
|||
Life span |
>3 years |
|||
Size |
Surface area m2/m3 |
Void volume % |
Packing density Kg/m3 |
|
Inch |
mm |
|||
1/2” |
16 |
260 |
91 |
80 |
1” |
25 |
210 |
92 |
79 |
1-1/2” |
38 |
140 |
94 |
58 |
2” |
50 |
100 |
94 |
54 |
3-1/2” |
90 |
73 |
96 |
33 |
Feature |
High void ratio, low pressure drop, low mass-transfer unit height, high flooding point, uniform gas-liquid contact, small specific gravity, high efficiency of mass transfer. |
|||
Advantage |
1. Their special structure make it has big flux, low pressure drop, good anti-impaction capability. |
|||
Application |
These various plastic tower packing are widely used in petroleum and chemical, alkali chloride, gas and environmental protection industries with max. temperature of 150°. |
Plastic tower packing can be made from heat resistant and chemical corrosion resistant plastics, including polyethylene (PE), polypropylene (PP), reinforced polypropylene (RPP), polyvinyl chloride (PVC), chlorinated polyvinyl chloride (CPVC), polyvinyiidene fluoride (PVDF) and Polytetrafluoroethylene (PTFE). The temperature in media ranges from 60 Degree C to 280 Degree C.
Performace/Material |
PE |
PP |
RPP |
PVC |
CPVC |
PVDF |
Density(g/cm3)(after injection molding) |
0.98 |
0.96 |
1.2 |
1.7 |
1.8 |
1.8 |
Operation temp.(℃) |
90 |
>100 |
>120 |
>60 |
>90 |
>150 |
Chemical corrosion resistance |
GOOD |
GOOD |
GOOD |
GOOD |
GOOD |
GOOD |
Compression strength(Mpa) |
>6.0 |
>6.0 |
>6.0 |
>6.0 |
>6.0 |
>6.0 |
Material
Our Factory assure all tower packing made from 100% Virgin Material.
1. OCEAN SHIPPING for large volume.
2. AIR or EXPRESS TRANSPORT for sample request.
Package type |
Container load capacity |
||
20 GP |
40 GP |
40 HQ |
|
Ton bag |
20-24 m3 |
40 m3 |
48 m3 |
Plastic bag |
25 m3 |
54 m3 |
65 m3 |
Paper box |
20 m3 |
40 m3 |
40 m3 |
Delivery time |
Within 7 working days |
10 working days |
12 working days |